PE420其具有较
了解更多联系:朱经理13823605771 13725867699 QQ865590763 ECTEE物性:
比重
|
1.68
|
|
ASTM D792
|
熔流率(熔体流动速率) (275°C/2.16 kg)
|
18
|
g/10 min
|
ASTM D1238
|
收缩率 - 流动
|
0.025
|
in/in
|
ASTM D955
|
吸水率 (平衡)
|
< 0.10
|
%
|
ASTM D570
|
洛氏硬度 (R 级)
|
90
|
|
ASTM D785
|
肖氏硬度 (邵氏 D)
|
75
|
|
ASTM D2240
|
拉伸模量 2 (73°F)
|
240000
|
psi
|
ASTM D638
|
抗张强度 2
|
|
|
ASTM D638
|
屈服, 73°F
|
4350
|
psi
|
|
断裂, 73°F
|
6820
|
psi
|
|
伸长率 2
|
|
|
ASTM D638
|
屈服, 73°F
|
5.0
|
%
|
|
断裂, 73°F
|
250
|
%
|
|
弯曲模量 3 (73°F)
|
245000
|
psi
|
ASTM D790
|
弯曲强度 3 (73°F)
|
6820
|
psi
|
ASTM D790
|
摩擦系数
|
|
|
ASTM D1894
|
与自身 - 动态
|
0.20
|
|
|
与自身 - 静态
|
0.20
|
|
|
泰伯耐磨性 (1000 Cycles, 500 g, CS-17 转轮)
|
5.00
|
mg
|
|
悬壁梁缺口冲击强度
|
|
|
ASTM D256
|
-40°F, 0.126 in
|
3.9
|
ft·lb/in
|
|
73°F, 0.126 in
|
无断裂
|
|
|
载荷下热变形温度
|
|
|
ASTM D648
|
66 psi, 未退火
|
194
|
°F
|
|
264 psi, 未退火
|
149
|
°F
|
|
脆化温度
|
< -105
|
°F
|
ASTM D746A
|
玻璃转化温度
|
185
|
°F
|
DMA
|
熔融温度
|
468
|
°F
|
ASTM D3418
|
结晶峰温度 (DSC)
|
432
|
°F
|
ASTM D3418
|
线形热膨胀系数 - 流动
|
5.6E-5
|
in/in/°F
|
ASTM D696
|
比热 (73°F)
|
0.230
|
Btu/lb/°F
|
ASTM D3418
|
导热系数 (104°F)
|
1.0
|
Btu·in/hr/ft²/°F
|
ASTM C177
|
结晶热
|
40.0
|
J/g
|
ASTM D3418
|
热稳定性 - 1%质量损失,N2
|
761
|
°F
|
TGA
|
融合热量
|
42.0
|
J/g
|
ASTM D3418
|
体积电阻率 4 (73°F)
|
5.5E+16
|
ohm·cm
|
ASTM D257
|
介电强度 (73°F, 0.126 in)
|
360
|
V/mil
|
ASTM D149
|
介电常数 (73°F, 1 MHz)
|
2.57
|
|
ASTM D150
|
UL 阻燃等级
|
V-0
|
|
UL 94
|
极限氧指数
|
52
|
%
|
ASTM D2863
|
|